Riblene GP 26 is a high fluidity low density polyethylene resin (LDPE). Main Applications: Riblene GP 26 is suitable for coating applications where low neck-in and high draw-down are key factors. For its excellent organoleptic properties Riblene GP 26 can be used for foodstuff flexible packaging. Moreover, for its rheological properties, Riblene GP 26 can be used for injection molded medium thickness articles, toys and houseware. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |