MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman DURACRYN 8080 NC Thermoplastic Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes:

Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80Instantaneous; ASTM D2240
Tensile Strength, Ultimate 2500 psiASTM D412
Elongation at Break 450 %ASTM D412
100% Modulus 0.800 ksi
@Strain 100 %
ASTM D412
Graves Tear Strength 300 pliDie C; ASTM D624; DIN 53507
Compression Set 67 %
@Temperature 70.0 °C
Method B, 22 hours; ASTM D395
 63 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395
Tensile Set 9.0 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Clash Berg Stiffness Temperature -18.0 °CAt 10,000 psi; ASTM D1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Engage® Polyolefin Elastomer
Dynasol Solprene® 4316 Thermoplastic Rubber (SBS)
Dow Engage® 8150 Polyolefin Elastomer
Dow Engage® 8180 Polyolefin Elastomer
Dow Engage® 8200 Polyolefin Elastomer

PAPA048 / 24115

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.