MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT HANSA AC 5610 Silicone Antifoam
Categories: Other Engineering Material

Material Notes: Description: Silicone antifoam for industrial agriculture applications.

Key Features

  • Low polarity
  • Good stability to water hardeners
  • Ready to use
  • Stable at pH 2-11
Key Applications
  • Agricultural adjuvant, antifoam
Application: High performing antifoam for agricultural formulations based on poyether modified siloxane. Low polarity. HANSA AC 5610 is a ready to use antifoam and can be easily diluted with water. The product can be used directly as a spray tank additive to control foaming during processing and application. The product also suitable for formulating antifoam products by diluting with water and stabilizing with thickeners. HANSA AC 5610 can be also used as a process additive during productions of chemicals for agriculture.

dosage recommendation:
ready to use: 0.01-0.30%
For antifoams formulations: 5 - 20%
As process additive: 0.01-0.30%

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccBS ISO 2781
Storage Temperature 5.00 - 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
% actives0.7
AppearanceWhite to yellowish liquid
ChemistryEmulsion of a polyether modified siloxane
ColorWhite to yellowish
IonicityNon-ionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL253 / 314736

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.