MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Aktiplast® PP Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Peptizer and processing promoter for elastomer compounds, especially based on natural rubber

Use: Aktiplast PP has a peptizing effect in NR and IR at mixing temperatures >60 °C. It retards scorch and accelerates vulcanization. Aktiplast PP decreases the viscosity of compounds based on NR resulting in an easier processing. This leads to higher extrusion rates, better dimensional stability and a constant level of die swell. Aktiplast PP provides a good dispersion of the fillers and rubber chemicals in the compound. Depending on the composition of the mixture, Aktiplast PP improves scorch behavior, promotes vulcanization and makes demolding much easier, leaving the mold clean.

Application: Tires, molded and extruded articles of all types, hard rubber

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/cc
Ash 12 - 14 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 101 - 111 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.5 Month
 
Descriptive Properties
Appearancelight brown Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8253 / 208646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.