MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Cristal™ One Pro Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Cristal™ One Pro is a copolyester designed to be fully compatible with the PET recycling stream. It enables recyclable cosmetics packaging that is tough and exhibits good chemical resistance. It is suitable for molding thick-walled transparent containers or parts (up to approximatively 12mm), while maintaining clarity and color. Cristal™ One Pro meets the definition of resin identification code #1 (RIC1) as defined by the California Assembly Bill (#906) and by ASTM D7611, Association of Plastic Recyclers (APR) as well as European PET Bottle Platform (EPBP). Other end-product attributes, including but not limited to size, color, auxiliary components, and availability of collection, may also impact recyclability.

Applications

  • Color cosmetics packaging
  • Fragrance packaging
  • Jars-skin care pkg
  • Personal care & cosmetics packaging
  • Skin care packaging
Key Attributes
  • Ability to mold thick parts
  • Excellent processing capabilities
  • Good chemical resistance
  • Good gate aesthetics
  • Good toughness
  • Recyclable with the PET stream
  • Transparency

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm0.00300 - 0.00500 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 54.0 MPa7830 psiASTM D638
Elongation at Break >= 150 %>= 150 %ASTM D638
Tensile Modulus 2.30 GPa334 ksiASTM D638
Flexural Yield Strength 78.0 MPa11300 psiASTM D790
Flexural Modulus 2.40 GPa348 ksiASTM D790
Izod Impact, Notched 0.520 J/cm0.974 ft-lb/inASTM D4812
Izod Impact, Unnotched NBNBASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C144 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 16.0 - 38.0 °C60.8 - 100 °F
Drying Temperature 130 - 140 °C266 - 284 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4041 / 323664

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.