MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM Cat Clear SP Condensation Cure Moldmaking Catalyst for QM 130T
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM Cat Clear SP is a fast curing, two-component, room temperature, condensation cure catalyst for QM 130T. The cured rubber has excellent mechanical properties and good shelf-life stability. QM Cat Clear is available for applications requiring a slower cure. Thixotropic and styrene resistant specialty catalysts are also available.

Key Features:

  • Excellent physical properties and dimensional stability
  • Fast demold time
Main Applications:
  • Vacuum bags
  • Molds for technical articles and prototypes
  • Spray applications

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccUncatalyzed
Viscosity 150 cPUncatalyzed
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 4.00 hourDemold time, Catalyzed
Tack-Free Time 1.00 - 2.00 hourCatalyzed
Pot Life <= 5.00 minCatalyzed
 
Descriptive Properties
ColorTranslucentUncatalyzed
 TranslucentCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PACC2065 / 199453

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.