MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nouryon Trigonox 44B VRN 3,5-Dimethyl-1,2-dioxolane-3,5-diol
Categories: Other Engineering Material

Material Notes: Trigonox 44B VRN is an acetylacetone peroxide formulation for fast curing of unsaturated polyester resins in the presence of a cobalt accelerator at room and elevated temperatures, including a Vanishing Red (VR) system.

CAS number: 13784-51-5

EINECS/ELINCS No: 253-384-9

Applications: Trigonox 44B VRN is an acetyl acetone peroxide formulation for the curing of unsaturated polyester resins in the presence of a cobalt accelerator at room and elevated temperatures. With the curing system Trigonox 44B VRN/cobalt accelerator a much faster speed of cure may be achieved than with curing systems based on a MEKP plus cobalt accelerator, at room and elevated temperatures. Normally the gel times with Trigonox 44B VRN are comparable to those with Butanox M- 50.Trigonox 44B VRN is particularly suitable in those applications where a fast mould-turnover is required, e.g. for the cold press moulding or resin injection moulding techniques.The system Trigonox 44B VRN/cobalt accelerator will give a higher peak exotherm than a standard MEKP/cobalt accelerator system. Due to this fact, is it recommendable to avoid the production of too thick laminates in one operation. At low temperatures a reasonable speed of cure is still obtained when Trigonox 44B VRN is used in combination with large amounts of cobalt accelerator possibly in combination with N,NDimethylaniline as promotor.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.055 g/cc0.03811 lb/in³
Viscosity 21 cP21 cP
Storage Temperature -10.0 - 25.0 °C14.0 - 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 60.0 °C140 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceRed liquid
Color<50 Pt-Co/ APHA
Content4.0-4.2 %Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1128 / 286651

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.