Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BRP Manufacturing Viton® V1630 Rubber Sheet
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Material: Viton® Rubber Sheet
BRP Style: V1630
Finish: Smooth or Nylon
ASTM Callout: M2HK710A1-10B37EO78Z1Z2,Z1 = 75 ± 5 duro Z2 DuPont Viton®

Information provided by BRP Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 10.0 MPa>= 1450 psiOriginal; ASTM D412
 6.998 - 13.00 MPa
@Temperature 250 °C,
Time 252000 sec
1015 - 1885 psi
@Temperature 482 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Elongation at Break 175 %175 %Original; ASTM D412
 <= 87.5 %
@Temperature 250 °C,
Time 252000 sec
<= 87.5 %
@Temperature 482 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Compression Set <= 50 %
@Temperature 175 °C,
Time 79200 sec
<= 50 %
@Temperature 347 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air 0.000 °C32.0 °F
 
Descriptive Properties
Hardness60-90Heat Aged, ASTM D573, 70 h @ 250°C
 70-80ASTM D2240
Oil Immersion<10% Volume ChangeASTM D471, IRM 903 Oil, 70 h @ 150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRPM057 / 315718

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.