Polifil® TPO-60D12UV is a UV stabilized injection molding grade of compounded TPO utilizing metallocene catalyst technology. This product is intended for applications requiring outstanding impact properties at both ambient and low temperatures needing UV stabilization. Typical applications include automotive bumper and fascia components, recreational vehicle cowls, and lawn and garden machinery guards.Information provided by The Plastics Group. |