NORYL GTX™ 934 resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits improved processability and excellent heat aging performance. NORYL GTX934 resin was designed for high heat automotive under-the-hood applications. Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Good Processability,Structural Information provided by SABIC |