MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Elantas CE-1171 (Conap) Acrylic Dielectric Conformal Coating
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Dielectric Conformal Coatings for Electronics
Cytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, instrumentation (industrial and military), missiles, spacecraft, fire and smoke detectors as well as coatings for electronic components, coils and transformers. And no small reason why -- all of the coatings described have been specifically formulated as dielectric insulating coatings to provide the user the ultimate protection available for his electronic assemblies; be it environmental (dirt, dust, humidity, fungus, temperature extremes, etc) or electrical insulation of conductors. These coatings are not designed for use as floor coatings or other general purpose uses; they have been produced under essentially "clean-room" conditions using raw materials with a minimum of ionizable impurities which would detract from their insulating qualities.

Cytec (Conap) CE-1171 Acrylic Dielectric Conformal Coating
  • Single Component
  • Passes Thermal Shock Test (MIL-I-46058C)
  • Non-Nutrient Fungus Resistance (MIL-I-46058C)
  • Passes Flexibility Test (1/8" Mandrel Bend) (MIL-I-46058C)
  • Poor Chemical and Solvent Resistance
  • Solvent Evaporation Cure
Cure Type: Solvent Evaporation

Information provided by Cytec, subsequently acquired by Elantas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 30 %30 %
Viscosity 850 cP
@Temperature 25.0 °C
850 cP
@Temperature 77.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmInsulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity)
 1.50e+16 ohm-cm1.50e+16 ohm-cmInitial Insulation Resistance (50% Relative Humidity)
 2.50e+12 ohm-cm
@Temperature 65.0 °C
2.50e+12 ohm-cm
@Temperature 149 °F
Insulation Resistance During 10th day Cycling (95% Relative Humidity)
Dielectric Constant 3.153.15ASTM D150
Dielectric Strength 118 kV/mm3000 kV/inASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 54.4 °C130 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
Flash Point 18.3 °C65.0 °F(TCC)
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 60.0 °C
1.00 hour
@Temperature 140 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Tack-Free Time 20.0 min
@Temperature 25.0 °C
0.333 hour
@Temperature 77.0 °F
Shelf Life 12.0 Month12.0 MonthShelf Life Time at 25°C in original, unopened containers.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCYTEC03 / 29235

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.