MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro SOFTCEL® VE-1100 Polyol
Categories: Other Engineering Material

Material Notes: Softcel VE-1100 polyether polyol is a unique polyol for the production of slabstock and molded viscoelastic foam.

Properties / Applications: Softcel VE-1100 polyether polyol is a unique polyol for the production of slabstock and molded viscoelastic foam. It provides expanded formulating and processing flexibility and is designed to offer enhanced reactivity and promote cure of high density viscoelastic foams. This allows for the production of a wide range of viscoelastic foam grades with consistent performance properties that can be tailored to end-use applications. Softcel VE-1100 is typically employed as the primary polyether polyol in TDI based formulations of most standard density and firmness grades of slabstock foams. Firm grades may require an addition of a high solids polymer such as Arcol® HS-100 polymer. Low level addition of a high hydroxyl foam modifier/extender is generally recommended to control foam recover rates. Most other standard chemical intermediates may be employed. Use of a lower functionality MDI such as Mondur® 3694 may be beneficial for processing very high density slabstock grades and is recommended for production of molded viscoelastic foam. As with any product, use of Softcel VE-1100 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.029 g/cc1.029 g/cc
Bulk Density 1.03 g/cc0.0372 lb/in³
Viscosity  125 cP
@Temperature 45.0 °C
125 cP
@Temperature 113 °F
 175 cP
@Temperature 35.0 °C
175 cP
@Temperature 95.0 °F
 240 cP
@Temperature 25.0 °C
240 cP
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point 212 °C414 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.030 %<= 0.030 %
 
Descriptive Properties
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0973 / 202756

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.