MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zotefoams Plastazote® LD45 Low Density Polyethylene Foam
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

Compliant with EC food contact and US FDA regulations.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0370 - 0.0470 g/ccsheet density
 0.0450 g/ccNominal skin/skin; BS ISO 7214 1998
Cell Length 0.400 mmTypical Diameter
 0.250 - 0.600 mm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 6010 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.560 MPaISO 7214 1998
Elongation at Break 175 %
Flexural Modulus 1.00 MPaBS4370, part 4, method 14
Compressive Yield Strength 0.0770 MPa
@Strain 10 %
BS ISO 7214 1998
 0.0940 MPa
@Strain 25 %
BS ISO 7214 1998
 0.130 MPa
@Strain 40 %
BS ISO 7214 1998
 0.170 MPa
@Strain 50 %
BS ISO 7214 1998
Tear Strength 1.15 kN/mBS EN ISO 8067 1995
Compression Set 2.5 %
@Time 79200 sec,
Strain 25 %
24 hr recovery; BS ISO 7214 1998
 7.5 %
@Time 79200 sec,
Strain 25 %
0.5 hr recovery; BS ISO 7214 1998
 10 %
@Time 79200 sec,
Strain 50 %
24 hr recovery; BS ISO 7214 1998
 18.5 %
@Time 79200 sec,
Strain 50 %
0.5 hr recovery; BS ISO 7214 1998
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0420 W/m-Kmean temp of 10°C; ISO 8302 1991
Maximum Service Temperature, Air 105 °C
Minimum Service Temperature, Air -70.0 °C
Flammability Test 0.70
@Thickness 13.0 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 1.3
@Thickness 5.00 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998
Shrinkage <= 1.0 %
@Temperature 70.0 °C
 <= 2.0 %
@Temperature 80.0 °C
 <= 3.0 %
@Temperature 90.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam
Zotefoams Plastazote® LD60 Low Density Polyethylene Foam
Zotefoams Plastazote® LD15 Low Density Polyethylene Foam
6060 Aluminum Composition Spec
Sawbones Solid Rigid Polyurethane Foam 10 pcf Density

PZOTEF919 / 150675

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.