MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Solvera® PT 5060 PFPE Surface Treatment
Categories: Fluid; Polymer

Material Notes: Solvera® PFPE is a sustainable surface treatment developed to increase the grease resistance of paper packaging, pizza boxes, popcorn bags, pet food bags and food wraps. Both solvent and aqueous formulations are available and can be diluted to any concentration with water. It complies with FDA regulations 21 CFR 176.180 and 21 CFR 176.170 and does not contain perfluoro-octanyl acid (PFOA) and perfluoro-octanyl sulfonate (PFOS) nor is it based on telomer chemistry.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
pH 7.0 - 9.0
Viscosity <= 300 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point 58.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
AppearanceAmber Dispersion
Dry Content (wt. %)25
Solvent Content (wt. %)<1DPM, di-propylene glycol methyl ether

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WAUSI551 / 149997

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.