MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Firelite LOD SW HT Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Soluble Glass Fiber raw material base. Hydraulic bond. An insulating concrete based on low bio-persistent fibres for service up to 1200°C/2200°F, expressly designed to withstand thermal shock; it has extremely low thermal conductivity. Particularly recommended for the following applications: by casting: special shapes to complete fibre lining of heaters and furnaces; kiln car tops for rapid firing in ceramic industry; by trowelling: lining of launders and distributors in primary aluminium industry; lining of ladles in secondary aluminium industry.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.980 g/cc0.0354 lb/in³dried to 110°C
Grain Size <= 10000 µm<= 10000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  1.20 MPa
@Temperature 815 °C
174 psi
@Temperature 1500 °F
 1.50 MPa
@Temperature 110 °C
218 psi
@Temperature 230 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.170 W/m-K
@Temperature 200 °C
1.18 BTU-in/hr-ft²-°F
@Temperature 392 °F
 0.200 W/m-K
@Temperature 400 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.220 W/m-K
@Temperature 600 °C
1.53 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Maximum Service Temperature, Air <= 1200 °C<= 2190 °F
Shrinkage 1.0 %1.0 %MST
 0.20 %
@Treatment Temp. 815 °C
0.20 %
@Treatment Temp. 1500 °F
 
Descriptive Properties
Net Material Required (kg/m³)900
Water Addition60-85% by weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6391 / 203175

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.