MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

M Cubed Technologies ASC-701 Aluminum alloy-70% SiC Metal Matrix Composite
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite

Material Notes: High stiffness, low density, low CTE composite. Components can be formed with complicated features, and can be machined to tight tolerances. Applications in high-precision equipment--semiconductor, automotive, aerospace.

Information provided by M Cubed Technologies, Inc.

Key Words: AlSiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.01 g/cc0.109 lb/in³ASTM C135
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 230 MPa33400 psiASTM E8
Modulus of Elasticity 270 GPa39200 ksiASTM E494
Flexural Strength 230 MPa33400 psiASTM C1161
Poissons Ratio 0.220.22ASTM E494
Fracture Toughness 10.0 MPa-m½9.10 ksi-in½ASTM C1421
Shear Modulus 111 GPa16100 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.20 µm/m-°C
@Temperature 25.0 - 100 °C
3.44 µin/in-°F
@Temperature 77.0 - 212 °F
ASTM E831
Thermal Conductivity 170 W/m-K1180 BTU-in/hr-ft²-°FASTM E1461
 
Descriptive Properties
MatrixAl Alloy
Particle ReinforcementSiC
Vol. % Reinforcement70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products
PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite
PCC-Advanced Forming Technology 68% AlSiC Metal Matrix Composite
M Cubed Technologies ASC-301 Aluminum alloy-30% SiC Metal Matrix Composite
M Cubed Technologies MMC-S55 Aluminum alloy-55% SiC Metal Matrix Composite

NMCUBE03 / 99803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.