MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Bada BADAMID® A70 GF30 FR HF uncolored (red phosphorus) Nylon 66, 35% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: 30% glass fiber filled, flame-protected with red phosphor, heat-stabilized injection molding grade with medium viscosity and very good electrical characteristics

Information provided by Bada

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183
Moisture Absorption 1.20 %50% r.h.; ISO 62
Water Absorption at Saturation 5.5 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 190 MPa
@Load 36.5 kg
ISO 2039-1
Tensile Strength at Break 150 MPa5 mm/min; ISO 527-1/2
Elongation at Break 3.0 %5 mm/min; ISO 527-1/2
Tensile Modulus 9400 MPa1 mm/min; ISO 527-1/2
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC-62631-3-1
Surface Resistance 1.00e+12 ohmIEC-62631-3-2
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC-62631-2-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC-62631-2-1
Comparative Tracking Index 600 VIEC-60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 28.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 65.0 µm/m-°CISO 11359-2
Melting Point 262 °C10 K/min; ISO 3146
Maximum Service Temperature, Air 220 °Csome hours; EC-60216
 130 °C
@Time 7.20e+7 sec
EC-60216
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 240 °CISO 75-1/2
Flammability, UL94 V-0
@Thickness 0.750 mm
 V-0
@Thickness 1.50 mm
Glow Wire Ignition Temperature 800 °C
@Thickness 1.00 mm
IEC-60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC-60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °C
Mold Temperature 80.0 - 90.0 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBADA066 / 286899

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.