MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
MarkeTech Zirconium Oxide Ceramic Zirconia, Tetragonal, Y2O3 Stabilized  (discontinued **)
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Data provided by the supplier, MarkeTech International.

Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is significantly improved. This makes some grades of zirconia superior to most materials for abrasion and wear resistance. Parts can be machined before firing in the green state and after firing to meet exacting specifications. Zirconia is electrically conductive above 900°C. Zirconia can be tape cast into very thin sheets for fuel cells and engineered ceramics.

MarkeTech International is no longer in business.

Key Words: ZrO2; YSZ; Yttria Stabilized Zirconia
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 1300kg/mm²
Modulus of Elasticity 205 GPa
Flexural Strength 1300 MPa
Compressive Strength 3900 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.9 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 2.30 W/m-K

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Yttria Stabilized Zirconia, YSZ
MarkeTech Zirconium Oxide Ceramic - Zirconia, Y2O3 Stabilized
Zirconium Oxide, Zirconia, ZrO2
MarkeTech Zirconium Oxide Ceramic, Zirconia MgO Stabilized
Magnesia Stabilized Zirconia

C5MT39 / 360

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.