1 inch wide, 30 mil thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number. Design/Construction: - Rubber: Cured self-fusing silicone rubber
- Cross-section: 1" wide rectangular
- Interleave: 2.5 mil Polyethylene
Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation. |