MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Titanium IMI 367 (Ti-6Al-7Nb)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Heat treatment: Anneal 1 hour at 700 °C, air cool.

Characteristics: High strength, alpha-beta alloy, excellent biocompatibility.

Applications: Femoral components for hip replacement.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.52 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 900 - 1000 MPa
Tensile Strength, Yield 800 - 900 MPa0.2% offset
Elongation at Break 12 %
Reduction of Area 35 %
Tensile Modulus 105 GPa
Fatigue Strength 500 MPa
@# of Cycles 1.00e+7
 
Thermal PropertiesOriginal ValueComments
Beta Transus 1010 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.5 - 6.5 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.0090 %
Iron, Fe <= 0.25 %
Nitrogen, N <= 0.050 %
Oxygen, O <= 0.20 %
Tantalum, Ta <= 0.50 %
Titanium, Ti 86 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V (Grade 5), STA
TIMET TIMETAL® 367 (Ti-6Al-7Nb) Implant Grade Titanium Alloy
Titanium Ti-5Al-2.5Fe ISO 5832/X Medical Grade
Titanium Ti-6Al-4V (Grade 5), Annealed Bar
Titanium Ti-6Al-4V (Grade 5), Annealed

MTP367 / 142961

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.