Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties. Films manufactured with Riblene FL 30 are easily heat shrinkable. Main Applications: Riblene FL 30 is recommended for general blown film applications, for the production of low gauge film and shrink film, for lamination and for blend. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |