MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 789-4 Thermally Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 789-4 one component, thermally conductive adhesive is designed for such applications as substrate attach, sealing micro-electronic packages, heat sink attach, and component staking. This adhesive provides four (4) times more thermal conductivity than unfilled epoxy adhesives. TRA-BOND 789-4 adhesive exhibits strong adhesion to difficult-to-bond metals, such as gold, silver, and copper. It retains its bond strength after exposure to moisture.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 75000 cPMixed (cp #51, 5 rpm)
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 3500 psiLap shear, alum to alum
 4000 psiLap shear, gold to gold
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+14 ohm-cm
Dielectric Constant 6.4
@Frequency 1000 Hz
Dielectric Strength 600 V/mil
Dissipation Factor 0.0010
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°CBelow Tg
 100 µm/m-°CAbove Tg
Thermal Conductivity 0.700 W/m-K
@Temperature 121 °C
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 130 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 125 °C
 30.0 min
@Temperature 150 °C
Shelf Life 6.00 MonthAt 5°C
 12.0 Month
@Temperature -40.0 °C
 
Descriptive Properties
Color Cream
Outgassing, NASA Passes
Weight Loss % 0.28At 250°C
Working Life, months 3At 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 972-1 Thermally Conductive Flexible Epoxy Adhesive
Tra-Con Tra-Bond Ablebond 744-2NTN1 Electrically Insulating Polyimide Adhesive
Tra-Con Tra-Bond Ablebond 933-1.5 Moisture Resistant Encapsulant
Tra-Con Tra-Bond Ablebond 862-2 Room Temperature Cure Epoxy Adhesive
Tra-Con Tra-Bond 968-5 High Dielectric Constant Epoxy Adhesive

PTRAC157 / 71085

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.