MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Tungsten Dispenser Cathodes
Categories: Other Engineering Material

Material Notes: 3M™ Tungsten Dispenser Cathodes typically consist of a porous tungsten matrix, impregnated with a barium based emission enhancing material. Depending on the application, this matrix may also be a mixed metal, such as tungsten iridium or tungsten molybdenum (for SEMBO cathodes). Dispenser cathodes are used in all types of vacuum devices, as well as in inert and reducing atmospheres. The most common applications include TWTs, klystrons, magnetrons and plasma devices.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 910 °C1670 °F
 
Descriptive Properties
Life Expectancy3000-15000 hr
Size0.25-200 mm
Tungsten Density Range74-84%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plansee W-10Cu Tungsten-Copper Composite
MarkeTech WCu10 Tungsten Copper Alloy
Cadi 10WA Tungsten Copper Alloy
3M 855 High Temperature Nylon Tape

PMM40029 / 194920

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.