MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Powersil® 415 MH Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® 415 MH is a high permittivity high consistency silicone rubber used for the production of refractive field control devices for cable accessories.

Properties:

  • silicone rubber with high permittivity
  • supplied ready-to-use
  • suitable for all types of molding applications
Application: The material is especially designed for the production of refractive field control devices for cable accessories.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183-1 A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 41ISO 868
Tensile Strength at Break 3.00 MPaISO 37
Elongation at Break 470 %ISO 37
Tear Strength 25.0 kN/mASTM 624 B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cmIEC 60250
Dielectric Constant 15IEC 60250
Dissipation Factor >= 0.15IEC 60250
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Powersil® 412 A/B Silicone Rubber
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer
Parker Chomerics CHO-MUTE 9005 Microwave Absorber
3M 5690K Silicone Rubber Termination Kits

PWACK9366 / 204895

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.