MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kolon SPELLOY® KD131 PC + ABS Alloy Resin  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.

High impact resistance (at low temperature), good dimensional stability, high heat resistance

Information provided by US distributor, API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccDIN 53479; ASTM D792
Water Absorption 0.20 %DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119DIN 53505; ASTM D785
Tensile Strength, Ultimate 610 kg(f)/cm²DIN 53455; ASTM D638
Elongation at Break 90 %DIN 53455; ASTM D638
Flexural Yield Strength 950 kg(f)/cm²DIN 53455; ASTM D790
Flexural Modulus 27000 kg(f)/cm²DIN 53452; ASTM D790
Izod Impact, Notched 55.0 kg-cm/cmDIN 53453; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.0
@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 25.0 kV/mmASTM D149/DIN 53481
Arc Resistance 124 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70 µm/m-°C
@Temperature 20.0 °C
DIN 53752; ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 110 °CDIN 53461; ASTM D648
Flammability, UL94 HB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PC/ABS + Stainless Steel
Chi Mei Wonderloy® PC-365 PC/ABS Alloy
Barlog Plastics KEBATER A0230 PBT/ABS, 30% glass fiber reinforced, low warpage
Avient Lubri-Tech™ BB-10GF/5T PC/ABS Blend, Glass Filled
Aquabond Technologies Aquabond™ ABS-55 Water Soluble Adhesive and Bonding Thermoplastic

PKOL090 / 48996

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.