MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Redwood Plastics Redco™ 60A Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: This unique formulation is stands up to abrasion and is resistant to deterioration in impingement applications. Redco™ 60A also performs well as a shock and vibration buffer while maintaining flexibility.

Standard Color: Blue

Features: Strong, Oil Resistant, Abrasion Resistant, Impact Resistant

Typical Applications: Impact wear liners, wear liners, roll covers, shock and vibration pads, rollers, carry over wheels, bumpers, wheels, flexible parts, impact pads, anti-vibration parts, wipers, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 57 - 6357 - 63
Tensile Strength 37.0 MPa5370 psi
Elongation at Break 650 %650 %
100% Modulus 2.60 MPa377 psi
300% Modulus 6.40 MPa928 psi
Resilience 6565DIN
Tear Strength 13.6 kN/m77.6 pliTrouser
 48.5 kN/m277 pliAngle, Die C
Abrasion 1515[mm3], DIN, 10N
Compression Set 31 %31 %Method B
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW026 / 296592

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.