PRE-ELEC PA 1406 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon fiber. In addition to a low electrical resistivity PRE-ELEC PA 1406 has an excellent balance of mechanical properties and is easy to injection mould. Typical applications include injection molded technical parts and housings for electronic components and other static sensitive devices (SSD) when high rigidity is needed. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod. Information provided by Premix Thermoplastics Inc. |