MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

EOS Titanium Ti64 Processed by DMSL on EOSINT M 270 and EOSINT M 280
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Description: Parts built in EOS Titanium Ti64 have a chemical composition corresponding to ISO 5832-3, ASTM F1472 and ASTM B348. This well-known light alloy is characterized by having excellent mechanical properties and corrosion resistance combined with low specific weight and biocompatibility. This material is ideal for many high-performance engineering applications, for example in aerospace and motor racing, and also for the production of biomedical implants (note: subject to fulfillment of statutory validation requirements where appropriate). Due to the layerwise building method, the parts have a certain anisotropy, which can be reduced or removed by appropriate heat treatment - see Technical Data for examples.

Heat treated at 800 °C (1470 °F) for 4 hours

Information provided by Proto3000

Key Words: Direct Metal Laser Sintering, Ti-6-4; UNS R56400; ASTM Grade 5 titanium; Ti6Al4V; Titanium Ti-6Al-4V
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.41 g/cc0.159 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 308 - 332308 - 332EN ISO 6507-1
Tensile Strength 980 - 1020 MPa142000 - 148000 psiin vertical direction (Z), Heat treated; ISO 6892-1:2009 (B) Annex D
 1030 - 1070 MPa149000 - 155000 psiin horizontal direction (XY), Heat treated; ISO 6892-1:2009 (B) Annex D
 1020 - 1120 MPa148000 - 162000 psiin vertical direction (Z), As built; ISO 6892-1:2009 (B) Annex D
 1180 - 1280 MPa171000 - 186000 psiin horizontal direction (XY), As built; ISO 6892-1:2009 (B) Annex D
Tensile Strength, Yield  980 - 1020 MPa
@Strain 0.2 %
142000 - 148000 psi
@Strain 0.2 %
in horizontal direction (XY), Heat treated; ISO 6892-1:2009 (B) Annex D
 980 - 1020 MPa
@Strain 0.2 %
142000 - 148000 psi
@Strain 0.2 %
in vertical direction (Z), Heat treated; ISO 6892-1:2009 (B) Annex D
 1010 - 1110 MPa
@Strain 0.2 %
146000 - 161000 psi
@Strain 0.2 %
in horizontal direction (XY), As built; ISO 6892-1:2009 (B) Annex D
 1020 - 1120 MPa
@Strain 0.2 %
148000 - 162000 psi
@Strain 0.2 %
in vertical direction (Z), As built; ISO 6892-1:2009 (B) Annex D
Elongation at Break 8.00 - 12.0 %8.00 - 12.0 %in horizontal direction (XY), As built; ISO 6892-1:2009 (B) Annex D
 8.00 - 14.0 %8.00 - 14.0 %in vertical direction (Z), As built; ISO 6892-1:2009 (B) Annex D
 13.0 - 15.0 %13.0 - 15.0 %in horizontal direction (XY), Heat treated; ISO 6892-1:2009 (B) Annex D
 14.0 - 16.0 %14.0 - 16.0 %in vertical direction (Z), Heat treated; ISO 6892-1:2009 (B) Annex D
Modulus of Elasticity 100 - 120 GPa14500 - 17400 ksiin horizontal direction (XY), As built; ISO 6892-1:2009 (B) Annex D
 100 - 120 GPa14500 - 17400 ksiin vertical direction (Z), As built; ISO 6892-1:2009 (B) Annex D
 104 - 124 GPa15100 - 18000 ksiin vertical direction (Z), Heat treated; ISO 6892-1:2009 (B) Annex D
 106 - 126 GPa15400 - 18300 ksiin horizontal direction (XY), Heat treated; ISO 6892-1:2009 (B) Annex D
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 350 °C662 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.50 - 6.75 %5.50 - 6.75 %
Titanium, Ti 88.75 - 91.0 %88.75 - 91.0 %Balance
Vanadium, V 3.50 - 4.50 %3.50 - 4.50 %
 
Descriptive Properties
Material composition< 2000 ppmO
 <150 ppmH
 <3000 ppmFe
 <500 ppmN
 <800 ppmC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NPROTO800 / 322913

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.