MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Parylene Coating Services C Poly (P-Xylylene)
Categories: Polymer; Thermoplastic; Poly (P-Xylylene)

Material Notes: Monomer is monochloro para-xylylene. Parylene C is recommended where excellent barrier protection is needed. It can be used up to 125°C where oxygen is present.

Parylene is a generic name for poly-para-xylylene polymers used as conformal coatings in protective applications.

The coating process exposes objects to the gas-phase monomer at low pressure. Through vacuum deposition, Parylene condenses on the surface in a polycrystalline fashion, providing a coating that is truly conformal and pinhole free.

Compared to liquid processes, the effects of gravity and surface tension are negligible -- so there is no bridging, thin-out, pinholes, puddling, run-off or sagging. And, since the process takes place at room temperature, there is no thermal or mechanical stress on the object.

Parylene is physically stable and chemically inert within its usable temperature range. Parylene provides excellent protection from moisture, salt spray, corrosive vapors, solvents, airborne contaminants and other hostile environments.

Property data obtained following ASTM methods. Information provided by Parylene Coating Services, Inc. (PCS)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.289 g/cc
Water Absorption 0.060 %0.029 inches; 24 hrs.
Moisture Vapor Transmission 0.140 cc-mil/100 in²-24hr-atm37°C; 90% RH
Oxygen Transmission 7.10 cc-mil/100 in²-24hr-atm23°C
Nitrogen Transmission 0.950 cc-mil/100 in²-24hr-atm23°C
Carbon Dioxide Transmission 7.70 cc-mil/100 in²-24hr-atm23°C
Hydrogen Sulfide Transmission 13.0 cc-mil/100 in²-24hr-atm23°C
Sulfur Dioxide Transmission 11.0 cc-mil/100 in²-24hr-atm23°C
Chlorine Transmission 0.350 cc-mil/100 in²-24hr-atm23°C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 10000 psi
Tensile Strength, Yield 8000 psi
Elongation at Break 200 %
Elongation at Yield 2.9 %
Tensile Modulus 3.20 GPa
Coefficient of Friction, Dynamic 0.29
Coefficient of Friction, Static 0.29
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+16 ohm-cm50% RH
Surface Resistance 1.00e+15 ohm50% RH
Dielectric Constant 2.95
@Frequency 1e+6 Hz
 3.1
@Frequency 1000 Hz
 3.15
@Frequency 60 Hz
Dielectric Strength 6800 V/milShort Time; 1 mil
Dissipation Factor 0.013
@Frequency 1e+6 Hz
 0.019
@Frequency 1000 Hz
 0.020
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.0820 W/m-K
Melting Point 290 °C
Maximum Service Temperature, Air 125 °CContinuous
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.639
Transmission, Visible 90 %Optically clear, but reports do not quantify.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating
Parylene Coating Services N Poly (P-Xylylene)
Parylene Coating Services D Poly (P-Xylylene)
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating

PPARYLC / 55911

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.