MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Polymaker PolyLite™ ABS 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: PolyLite™ ABS is made with a specialty bulk-polymerized ABS resin, which has significantly lower volatile content compared to traditional ABS resins. It delivers excellent printing quality with minimal odor during printing.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183, GB/T 1033
Moisture Absorption at Equilibrium 0.35 %
@Temperature 23.0 °C
0.35 %
@Temperature 73.4 °F
70% RH
Melt Flow 9.0 - 14 g/10 min
@Load 1.16 kg,
Temperature 220 °C
9.0 - 14 g/10 min
@Load 2.56 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272
Tensile Strength 25.4 MPa3680 psiZ Direction, Dry; ISO 527, GB/T 1040
 33.3 MPa4830 psiX-Y Direction, Dry; ISO 527, GB/T 1040
Elongation at Break 2.4 %2.4 %Z Direction, Dry; ISO 527, GB/T 1040
 2.7 %2.7 %X-Y Direction, Dry; ISO 527, GB/T 1040
Modulus of Elasticity 1.835 GPa266.1 ksiZ Direction, Dry; ISO 527, GB/T 1040
 2.174 GPa315.3 ksiX-Y Direction, Dry; ISO 527, GB/T 1040
Flexural Strength 72.8 MPa10600 psiX-Y Direction, Dry; ISO 178, GB/T 9341
Flexural Modulus 2.844 GPa412.5 ksiX-Y Direction, Dry; ISO 178, GB/T 9341
Charpy Impact, Notched 1.05 J/cm²5.00 ft-lb/in²ISO 179, GB/T 1043
 1.26 J/cm²6.00 ft-lb/in²ISO 179, GB/T 1043
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature 113.5 °C236.3 °F10°C/min; DSC
Deflection Temperature at 0.46 MPa (66 psi) 99.2 °C211 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 98.2 °C209 °FISO 75
Vicat Softening Point 103.9 °C219.0 °FISO 306, GB/T 1633
Glass Transition Temp, Tg 101.1 °C214.0 °F10°C/min; DSC
Decomposition Temperature >= 380 °C>= 716 °F10°C/min; DSC
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 264 °C473 - 507 °F
 
Descriptive Properties
Bed temperature (°C)90 - 100
Build surface materialBuildTak®
Printing speed (mm/s)30-50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYMA973 / 291038

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.