MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics BTU-Block ™ Flexible Thermal Ceramic
Categories: Ceramic

Material Notes: BTU-BLOCK Flexible is comprised of the microporous material enclosed in a high temperature textile and quilted to form a flexible sheet. Product Line Overview The BTU-BLOCK product line of microporous insulation is designed for use in high temperature industrial applications. BTU-BLOCK uses an optimized blend of raw materials to produce an insulation material with a uniquely low thermal conductivity. Unlike traditional fiber or ceramic based insulation, microporous insulation is based on ultra-fine particles of fumed silica, metal oxides and reinforcement fibers. These particles and fibers create a sub-micron pore structure that limits the convection of air, the conduction of heat, and the transmission of radiation. BTU-BLOCK insulation is designed to provide ultra-low thermal properties throughout the entire temperature range.

Applications: Back-up insulation in high temperature production processes, Molten metal ladles, Holding furnaces, Transfer ladles, Launders, Tundishes, Pipe wraps, Commercial ovens

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 1.08 MPaat 16 pcf, 10% deformation; ASTM C165
 1.85 MPaat 16 pcf, 20% deformation; ASTM C165
 2.85 MPaat 16 pcf, 30% deformation; ASTM C165
 4.62 MPaat 16 pcf, 40% deformation; ASTM C165
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0300 W/m-K
@Temperature 260 °C
ASTM C201
 0.0500 W/m-K
@Temperature 538 °C
ASTM C201
 0.0800 W/m-K
@Temperature 871 °C
ASTM C201
 0.0900 W/m-K
@Temperature 982 °C
ASTM C201
Maximum Service Temperature, Air <= 982 °Ccore material
Shrinkage 0.30 %
@Treatment Temp. 538 °C,
Time 86400 sec
ASTM C356
 0.60 %
@Treatment Temp. 815 °C,
Time 86400 sec
ASTM C356
 1.3 %
@Treatment Temp. 954 °C,
Time 86400 sec
ASTM C356

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool Millboard 822 Thermal Ceramic
Thermal Ceramics Alfibond 2100 Shapes
Morgan Advanced Ceramics Ceramic Fiber Blankets Cerawool Blanket
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Morgan Advanced Ceramics AL 1009™ Mac-A100W-Porous Aluminum Oxide Ceramic

CMORF6124 / 202908

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.