MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® X7099 BK V307171 Nylon 612, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass Fiber Filler

Material Notes: VESTAMID® X7099 BK V307171 is a PA 612 resin especially developed for the production of plastic-rubber composites. Parts made from VESTAMID® X7099 BK V307171 can be, without the use of adhesives or adhesion promoters, covulcanized with rubbers, such as XNBR, HNBR, AEM or FPM ("direct-bonding to rubber"). As a partially crystalline resin VESTAMID® X7099 BK V307171 exhibits an outstanding chemical resistance, especially against fuels, oils and fats. In comparison to resins based on PA 66 or PA 6 VESTAMID® X7099 BK V307171 has a distinctly lower water absorption. VESTAMID® X7099 BK V307171 is supplied as cylindrical pellets ready for use in a moisture-proof packaging. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Automotive and Mobility, Sustainable
Sustainability Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Oil / fuels
Additives: Glass fibers
Special Characteristics: Semi-crystalline, High heat resistant
Color: Black
Additives: Heat stabilizer
Chemical Resistance: Grease resistance, Oil resistance, Fuel resistance, General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Water Absorption 2.00 %Sim to ISO 62
Moisture Absorption 0.800 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00600 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0110 cm/cmISO 294-4, 2577
Melt Flow 10.0 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPaISO 527
Tensile Strength 125 MPaISO 527
Tensile Strength, Yield 125 MPaISO 527
Elongation at Break 5.00 %Nominal; ISO 527
Elongation at Yield 4.00 %ISO 527
Tensile Modulus 6000 MPaISO 527
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C(P); ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 62631-3-1
Dielectric Constant 3.90
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 4.40
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 38.0 kV/mmAC, S20/P50; Sim. To IEC 60243-1
Dissipation Factor 0.0430
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.0650
@Frequency 100 Hz
IEC 62631-2-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 215 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °CISO 75-1/-2
Vicat Softening Point 210 °C
@Load 5.10 kg
50 K/h; ISO 306
 215 °C
@Load 1.02 kg
50 K/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 80.0 °CInjection Molding; ISO 294
Injection Velocity 200 mm/secInjection Molding; ISO 294
Hold Pressure 70.0 MPaInjection Molding; ISO 274
 
Descriptive Properties
Blue water consumption20.5 kgISO 14040, 14044
ColorBlack
Global Warming Potential2.2 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.6 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 5.6 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7940 / 325072

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.