MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shin-Etsu Silicones LIMS™ KE2004-10A/B Elastomer
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes:

Information Provided by Shin-Etsu Silicones of America, Inc.

Key Words: LSR, Liquid Silicone Rubber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Viscosity 800000 cP800000 cPB
 1.30e+6 cP1.30e+6 cPA
Linear Mold Shrinkage 0.023 cm/cm0.023 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9.09.0
Tensile Strength 2.80 MPa406 psi
Elongation at Yield 580 %580 %
100% Modulus 0.179 MPa
@Strain 100 %
26.0 psi
@Strain 100 %
Tear Strength 10.0 kN/m57.1 pli
Compression Set 22 %
@Temperature 150 °C,
Time 3600 sec
22 %
@Temperature 302 °F,
Time 1.00 hour
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Temperature 120 °C
0.167 hour
@Temperature 248 °F
Press Cure
 
Descriptive Properties
AppearanceTranslucent
Cure Rate24T10 (302°F, ODR)
 51T90 (302°F, ODR)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos Nova 3101 General Purpose Crystal Polystyrene
I. Stern N2560 General Purpose Crystal Polystyrene
Eastman Eastar 6763 PETG Copolyester
Dow AIM® 4800 High Impact Styrenic Resin
Chevron Phillips MA9545 HIPS - High Impact Polystyrene

PSHIN032 / 103859

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.