MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness. HD-7756 is particularly recommended for films less than 0.5 mil in thickness.

Applications: Retail carry-out sacks; Merchandise bags; Institutional can liners; Consumer trash bags. Data for film properties below based on 0.5 mil film.

Key Words: High Density Polyethylene; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9535 g/cc0.03445 lb/in³Exxon Method
Thickness 12.7 microns0.500 mil
Melt Flow 0.055 g/10 min0.055 g/10 minExxon Method (I2). HLMI (I21) is 9 g/10 min.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 42.0 MPa6090 psiASTM D882
Film Tensile Strength at Yield, TD 34.0 MPa4930 psiASTM D882
Film Elongation at Break, MD 270 %270 %ASTM D882
Film Elongation at Break, TD 430 %430 %ASTM D882
Secant Modulus, MD 1.285 GPa186.4 ksiASTM D882
Secant Modulus, TD 1.415 GPa205.2 ksiASTM D882
Elmendorf Tear Strength, MD 0.394 g/micron10.0 g/milASTM D1922
Elmendorf Tear Strength, TD 5.51 g/micron140 g/milASTM D1922
Dart Drop 16.9 g/micron430 g/milF50; ASTM D-1709
Film Tensile Strength at Break, MD 95.0 MPa13800 psiASTM D882
Film Tensile Strength at Break, TD 66.0 MPa9570 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 °C264 °FExxon Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin
ExxonMobil Escorene® HD-7745 HMW-HDPE Blown Film Resin
ExxonMobil HTA 108 High Density Polyethylene Resin
ExxonMobil HTA 001HP2 High Density Polyethylene (HMW) Resin
ExxonMobil HTA 001HD High Density Polyethylene (HMW) Resin

PEXCG8 / 37956

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.