MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Thermal Ceramics 1302 Board and Shapes Molded Min-K Insulation
Categories: Ceramic

Material Notes: Min-K 1302 is a microporous material specifically designed to be molded into block and machined to specific customer designs. Min-K 1302 can also be supplied in blocks or boards.

Features:

  • Microporous
  • Low thermal conductivity
  • Compression resistant
  • Machined to customer specification
  • Lightweight
  • Organic
  • Applications:

  • Aerospace
  • High temperature
  • Thermoelectric devices
  • Instrumentation and analytical equipment
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.320 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Transverse Strength >= 55.0 psi
    Compressive Yield Strength 0.758 MPa5% compression
     1.31 MPa8% compression
     
    Thermal PropertiesOriginal ValueComments
    Specific Heat Capacity 0.230 BTU/lb-°F
    @Temperature 204 °C
     0.250 BTU/lb-°F
    @Temperature 427 °C
     0.270 BTU/lb-°F
    @Temperature 649 °C
     0.270 BTU/lb-°F
    @Temperature 871 °C
    Thermal Conductivity 0.200 BTU-in/hr-ft²-°F
    @Temperature 149 °C
     0.220 BTU-in/hr-ft²-°F
    @Temperature 204 °C
     0.230 BTU-in/hr-ft²-°F
    @Temperature 316 °C
     0.250 BTU-in/hr-ft²-°F
    @Temperature 427 °C
     0.270 BTU-in/hr-ft²-°F
    @Temperature 538 °C
     0.370 BTU-in/hr-ft²-°F
    @Temperature 649 °C
     0.520 BTU-in/hr-ft²-°F
    @Temperature 871 °C
    Maximum Service Temperature, Air 1800 °F
    Shrinkage 0.50 %
    @Temperature 982 °C,
    Time 14400 sec

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Thermal Ceramics 2800 RPC Shapes
    Thermal Ceramics TE 1400 Board and Shapes Molded Min-K Insulation
    Thermal Ceramics TE 1800 Board and Shapes Molded Min-K Insulation
    Sandvik Nisil Thermocouple Alloy
    Sandvik Nicrosil Thermocouple

    CTHERM207 / 2527

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.