MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Leaded Copper, UNS C18700, H04 Temper 25 mm rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Good cold workability, poor hot workability.

Applications: connectors, motor and switch parts, screw machine parts requiring high conductivity.

Test specimen: rod - 25mm diameter.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 5050
Tensile Strength, Ultimate 350 MPa50800 psi
Tensile Strength, Yield 315 MPa45700 psi
Elongation at Break 14 %14 %in 50 mm.
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.300.30Calculated
Machinability 85 %85 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Shear Strength 195 MPa28300 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000179 ohm-cm
@Temperature 20.0 °C
0.00000179 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.78 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 377 W/m-K
@Temperature 20.0 °C
2620 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 950 - 1080 °C1740 - 1980 °F
Solidus 950 °C1740 °F
Liquidus 1080 °C1980 °F
Annealing Point 427 - 649 °C800 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 650 °C797 - 1200 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99 %99 %
Lead, Pb 0.80 - 1.5 %0.80 - 1.5 %
Other, total <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C18900
Copper-Nickel-Phosphorus-Tellurium alloy, UNS C19100
Copper-Nickel-Phosphorus alloy, UNS C19000
Copper, UNS C19700, H08 Temper
Copper, UNS C19520, H12 Temper

MC18700b5 / 10922

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.