3M™ Dyneon™ Fluoroplastic Powder PFA 6503PAZ is a fluorothermoplastic powder designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tank liners, electrical insulation and low friction applications.Features and Benefits:- Excellent electrostatics
- Excellent non-stick performance
- Outstanding flow and fluidization
- Good stress crack resistance
- Smooth surfaces
- Good transparency
- Non-wetting
- Heat resistant to 260°C (500°F)
- Low friction
- Chemical resistance
- Process target: powder coating
This product complies with 21 CFR 177.1550 FDA regulationsInformation provided by the Dyneon division of 3M. |