MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Teijin Films Mylar® WRL63 Polyester Film, 200 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® WRL63 is a biaxially oriented polyester (OPET) film with a modified ethylene acrylate heat seal layer. It provides peelable seal over a broad temperature range to a number of bottles or containers including PET, PVC, PS, PE, and PP.

Mylar® WRL63 is a general purpose sealant product designed to produce good heat seals to substrates including polyethylene (PE), polypropylene (PP), amorphous polyester (APET, also PETG), semi-crystalline polyester (CPET), polyester coated paperboard, polyvinylchloride (PVC), and polystyrene (HIPS). Mylar® WRL63 has low heat seal initiation temperature and can be sealed over a wide temperature range. This allows good seals to be made at higher line speeds (or using lower sealing temperatures). Peelability and cleanness of the peel make Mylar® WRL63 ideal for the dairy market and the induction seal cap liner market.

FDA Food Contact Status - The above mentioned films comply with Food and Drug Administration Regulations 21 CFR 177.1630 -- Polyethylene Phthalate Polymers, subject to the limitations and requirements therein. This film may be used in contact with food under Conditions of Use C through H (as described in Table 2 of 21 CFR 176.170(c)), subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (c) of the Regulation. The conditions of use include hot fill or pasteurized above 150°F, refrigerated storage, frozen storage, and ready prepared foods intended to be reheated in container at time of use.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³Typical Mylar®; ASTM D1505
Water Vapor Transmission 15.5 g/m²/day
@Temperature 38.0 °C
1.00 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM F1249
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 %150 %ASTM D882A
Film Elongation at Break, TD 80 %80 %ASTM D882A
Film Tensile Strength at Break, MD 145 MPa21000 psiASTM D882A
Film Tensile Strength at Break, TD 221 MPa32000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)2.5 cc/100 in2O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal)9300 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 142 Gauge
DuPont Teijin Films Mylar® X842 Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge
DuPont Teijin Films Mylar® P25T Polyester Film, 50 Gauge
DuPont Teijin Films Mylar® P25 Polyester Film, 50 Gauge

PDTZ9440 / 139757

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.