MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Materion WS217 Solder
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Material Notes: Available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.

Former product of Williams Advanced Alloys. Williams Advanced Alloys is now a part of Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.73 g/cc0.279 lb/in³
 7.73 g/cc0.279 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 103 MPa15000 psi
Tensile Strength, Ultimate 103 MPa15000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00001686 ohm-cm0.00001686 ohm-cm
 0.0000169 ohm-cm0.0000169 ohm-cm10.2% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.0 µm/m-°C
@Temperature 20.0 °C
7.78 µin/in-°F
@Temperature 68.0 °F
 14.0 µm/m-°C
@Temperature 20.0 °C
7.78 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 28.0 W/m-K194 BTU-in/hr-ft²-°F
 28.0 W/m-K194 BTU-in/hr-ft²-°F
Melting Point 217 °C423 °F
Solidus 217 °C423 °F
Liquidus 217 °C423 °F
 
Component Elements PropertiesMetricEnglishComments
Gold, Au 10 %10 %
Tin, Sn 90 %90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indium Corp. Fine ITO Indium Tin Oxide
Materion WS118 Solder
Materion WS145 Solder
Materion WS179 Solder
Materion WS181 Solder

NWILL55 / 19943

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.