MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

SABIC LNP™ STAT-KON™ RD000I Nylon 66 (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Carbon Fiber Filled

Material Notes: LNP STAT-KON RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.0 MPa6670 psiASTM D638
Elongation at Break 13.5 %13.5 %ASTM D638
Flexural Strength 82.0 MPa11900 psiASTM D790
Flexural Modulus 2.62 GPa380 ksiISO 178/1A
Izod Impact, Notched 2.50 J/cm4.68 ft-lb/inASTM D256
Izod Impact, Unnotched 21.89 J/cm41.01 ft-lb/inASTM D4812
Tangent Modulus 2380 MPa345000 psi50 mm/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.0 - 6.0 ohm1.0 - 6.0 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 121 µm/m-°C
@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E 831
Thermal Conductivity 2.80 W/m-K19.4 BTU-in/hr-ft²-°FASTM E 1530
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
@Thickness 3.20 mm
167 °F
@Thickness 0.126 in
unannealed; ASTM D648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI22483 / 215619

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.