MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay FM® 6604-1 BMI Foaming Adhesive
Categories: Polymer; Adhesive; Thermoset; Bismaleimide (BMI)

Material Notes: Description: FM® 6604-1 is a modified bismaleimide (BMI) resin core splice foaming adhesive. It has a cure temperature of 350°F (177°C) with a post-cure at 440°C (227°C). The service temperature is -67°F to 450°F (-57°C to 232°C) with post-cure.

Features & Benefits:

  • Maximum continuous service temperature up to 450°F (232°C) with post-cure
  • Expansion ratio 2:1 nominal
  • Ideal for non-metallic core splice and edge closeout
  • Long-term aging
  • Fuel tight
  • High strength-to-density ratio
  • Structural equivalency to unspliced core
Applications:
  • Core shear-ties
  • Edge closeouts
  • Insert bonding

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.480 g/cc
Volatiles <= 2.0 %
Storage Temperature -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 260 psi
@Temperature 232 °C
Beam
 320 psi
@Temperature 204 °C
Beam
 530 psi
@Temperature 232 °C
Tube
 550 psi
@Temperature 24.0 °C
Beam
 630 psi
@Temperature -55.0 °C
Beam
 640 psi
@Temperature 204 °C
Tube
 900 psi
@Temperature 24.0 °C
Tube
 950 psi
@Temperature -55.0 °C
Tube
 1000 psi
@Temperature 24.0 °C
Tube, 1,1,1 trichloroethane soak per MIL-T-81533 vapor
 1300 psi
@Temperature 24.0 °C
Tube, 30-day salt spray per ASTM B-117 at 95°F (35°C)
 1400 psi
@Temperature 24.0 °C
Tube, 72-hour water boil in demineralized water
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 232 °C
Minimum Service Temperature, Air -57.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive
Evonik Compimide® TM123 4,4'-Bis(o-propenylphenoxy)benzophenone
Solvay HTM® 556 BMI
Henkel Hysol EA 9673 (BMI) Film Adhesive
Evonik Compimide® 353A Bismaleimide

PCYTED045 / 180347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.