MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SCG Chemicals P901J Homopolymer polypropylene resin
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: SCG PP P901J is a homopolymer polypropylene resin with excellent flow ability, high stiffness and high clarity. This grade is especially suitable for thin wall injection molding for food, beverage and general packaging.

Applications: Thin wall food and beverage packaging; - Food containers with high stiffness - Drinking cups with high clarity General thin wall products House wares.

Features: Excellent flow ability and high productivity. High clarity. High stiffness.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccASTM D 1505
Linear Mold Shrinkage, Flow 0.010 in/in
@Thickness 2.00 mm
TPE Method
Linear Mold Shrinkage, Transverse 0.0125 in/in
@Thickness 2.00 mm
TPE Method
Melt Flow 60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 1620 MPaASTM D790
Izod Impact, Notched 38.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 125 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 35 %ASTM D1003
 
Descriptive Properties
AppearancePellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC785 / 278042

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.