LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has corona treatment with a low sealing temperature. It is widely used in food and confectionary packaging with a low heat sealing temperature requirement.Information provided by Kinlead. |