MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Danquinsa DANCOLL® 245-35 PUR adhesive primer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCOLL® 245-35 is an 20% PUR adhesive primer based on a linear, hydroxyle group containing polyurethane. It is an optimum binder for many different structured textile supporting materials. It provides very good adhesive characteristics by the ground coat/impregnation of polyester- and polyamid fabrics. DANCOLL® 245-35 is used for laminations at the production of conveyor belts.

Application: DANCOLL® 245-35 is used as a PUR-primer for spread-, rotary printing and spray application which will be applied as a lamination adhesive, primer barrier coating or as an adhesive aid for a later lamination. As ground coat respective impregnation of textiles it is used for the later coating with PVC and TPU. It is suitable to serve as external coating for textile fire hoses and for the adhesive bonding of fire hose in-liners (Manchons) by the production of fire hoses. DANCOLL® 245-35 is distinguished by a tack-free drying process. The coated substrate should be cooled down well prior to its winding up as the substrate might bond due to residual heat.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³DIN 51.757
Solids Content 34 - 36 %34 - 36 %DIN 53.189
Viscosity 15000 - 30000 cP15000 - 30000 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point -3.00 °C26.6 °FDIN 51.755
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Aspectcolorless liquid
SolventEthyl acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ023 / 294443

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.