System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Armstrong A-1/V Epoxy Adhesive
Categories:
Polymer
;
Adhesive
;
Thermoset
;
Epoxy
;
Epoxy Adhesive
Material Notes:
A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°F
Information provided by Ellsworth Adhesives.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Viscosity
400000
cP
400000
cP
Mixed
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
83
83
Tensile Strength, Ultimate
37.9
MPa
5500
psi
after optimum cure
Elongation at Break
2.0 %
2.0 %
Adhesive Bond Strength
51.4
MPa
7450
psi
Steel-Steel; after optimum cure
15.9
MPa
@Temperature 82.2 °C
2300
psi
@Temperature 180 °F
Aluminum-Aluminum tensile shear
19.3
MPa
@Temperature -54.4 °C
2800
psi
@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
19.7
MPa
@Temperature 25.0 °C
2850
psi
@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Thermal Properties
Metric
English
Comments
CTE, linear
34.0
µm/m-°C
@Temperature 20.0 °C
18.9
µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air
121
°C
250
°F
Glass Transition Temp, Tg
77.0
°C
171
°F
Processing Properties
Metric
English
Comments
Processing Temperature
22.2
°C
72.0
°F
73.9
°C
165
°F
Optimum cure is 30 min. @ 165°F
149
°C
300
°F
Fast cure is 10 min. @ 300°F
Pot Life
<=
120
min
@Temperature 25.0 °C
<=
120
min
@Temperature 77.0 °F
100 g
Descriptive Properties
Color
Brown
Mix Ratio
4/1
By Weight
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified
Armstrong A-12 Epoxy Adhesive, at 1:1 Mix Ratio
Abatron AboCast 8504-5 One-Component Epoxy
Armstrong A-2/A Epoxy Adhesive
Armstrong A-12 Epoxy Adhesive, at 3:2 Mix Ratio
PARM02 / 24534
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.