Description: ACC18 is a fast curing, low viscosity, 1-component, condensation curing silicone coating. The uncured product can be applied by pouring, brushing or spraying and is readily cured to a tough, transparent rubber. It can be used to coat printed circuit boards to prevent ingress of water and environmental contaminants. Key Features - Fast Room temperature cure
- Low viscosity
- Fluorescent UV aid for Production QA checks
- Excellent adhesion to many substrates
- Excellent adhesion to Humiseal 1.94V-0 boards
- Low odor
- RoHS compliant
Cured Elastomer: After 7 days at 23°C / 55 +/- 5% Humidity on a 3 mm thick test sheetInformation provided by CHT Group |