MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Lord Cyanoacrylate Adhesives
Lord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metals and plastics. Lord Cyanoacrylate Adhesives offer these benefits: Instant Cure. Lord Cyanoacrylate Adhesives develop strong bonds with setting times ranging from 5 to 130 seconds. Ease of Use. Lord Cyanoacrylate Adhesives are one-component systems that facilitate set-up and minimize production costs. Good Environmental Resistance. Lord Cyanoacrylate Adhesives offer excellent resistance to weathering and aging.

Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate Adhesive
Fast setting. High elasticity. Low viscosity. Colorless adhesive for bonding plastic-to-metal and plastic-to-rubber. Very effective in bonding substrates with differing coefficients of expansion. MIL-A-46050C Type II, Class 1 Approved.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0382 lb/in³
Viscosity 30 cP30 cP
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0333 - 0.0667 min0.000556 - 0.00111 hourPlastic set time
 0.0333 - 0.0667 min0.000556 - 0.00111 hourRubber set time
 0.250 - 0.417 min0.00417 - 0.00694 hourMetal set time

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cesium, Cs
Bohrium, Bh
Actinium, Ac
Henkel Loctite® 420 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® 417 General Purpose Ethyl Cyanoacrylate Bonding Adhesive

PLORDAD54 / 52036

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.