MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Aluminum Bronze D, UNS C61400, Annealed Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot and cold formability.

Applications: nuts, bolts, stringers and threaded members, corrosion resistant vessels and tanks, structural components, machine parts, condenser tube and piping systems, marine protective sheathing and fasteners, munitions mixing troughs and blending chambers.

Key Words: CDA 614
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.89 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  50
@Load 3000 kg,
Temperature 538 °C
50
@Load 6610 lb,
Temperature 1000 °F
 84
@Load 3000 kg,
Temperature 427 °C
84
@Load 6610 lb,
Temperature 801 °F
 134
@Load 3000 kg,
Temperature 316 °C
134
@Load 6610 lb,
Temperature 601 °F
 142
@Load 3000 kg,
Temperature 204 °C
142
@Load 6610 lb,
Temperature 399 °F
 155
@Load 3000 kg,
Temperature 20.0 °C
155
@Load 6610 lb,
Temperature 68.0 °F
 161
@Load 3000 kg,
Temperature -29.0 °C
161
@Load 6610 lb,
Temperature -20.2 °F
 162
@Load 3000 kg,
Temperature -60.0 °C
162
@Load 6610 lb,
Temperature -76.0 °F
 185
@Load 3000 kg,
Temperature -182 °C
185
@Load 6610 lb,
Temperature -296 °F
Tensile Strength, Ultimate  92.0 MPa
@Temperature 538 °C
13300 psi
@Temperature 1000 °F
 174 MPa
@Temperature 427 °C
25200 psi
@Temperature 801 °F
 427 MPa
@Temperature 316 °C
61900 psi
@Temperature 601 °F
 522 MPa
@Temperature 204 °C
75700 psi
@Temperature 399 °F
 583 MPa
@Temperature 20.0 °C
84600 psi
@Temperature 68.0 °F
 600 MPa
@Temperature -29.0 °C
87000 psi
@Temperature -20.2 °F
 610 MPa
@Temperature -60.0 °C
88500 psi
@Temperature -76.0 °F
 707 MPa
@Temperature -182 °C
103000 psi
@Temperature -296 °F
Tensile Strength, Yield  68.0 MPa
@Strain 0.5 %,
Temperature 538 °C
9860 psi
@Strain 0.5 %,
Temperature 1000 °F
 123 MPa
@Strain 0.5 %,
Temperature 427 °C
17800 psi
@Strain 0.5 %,
Temperature 801 °F
 256 MPa
@Strain 0.5 %,
Temperature 316 °C
37100 psi
@Strain 0.5 %,
Temperature 601 °F
 276 MPa
@Strain 0.5 %,
Temperature 204 °C
40000 psi
@Strain 0.5 %,
Temperature 399 °F
 288 MPa
@Strain 0.5 %,
Temperature 20.0 °C
41800 psi
@Strain 0.5 %,
Temperature 68.0 °F
 303 MPa
@Strain 0.5 %,
Temperature -29.0 °C
43900 psi
@Strain 0.5 %,
Temperature -20.2 °F
 305 MPa
@Strain 0.5 %,
Temperature -60.0 °C
44200 psi
@Strain 0.5 %,
Temperature -76.0 °F
 347 MPa
@Strain 0.5 %,
Temperature -182 °C
50300 psi
@Strain 0.5 %,
Temperature -296 °F
Elongation at Break  30 %
@Temperature 316 °C
30 %
@Temperature 601 °F
 34 %
@Temperature 204 °C
34 %
@Temperature 399 °F
 36 %
@Temperature 538 °C
36 %
@Temperature 1000 °F
 44 %
@Temperature -29.0 °C
44 %
@Temperature -20.2 °F
 45 %
@Temperature 20.0 °C
45 %
@Temperature 68.0 °F
 47 %
@Temperature -60.0 °C
47 %
@Temperature -76.0 °F
 52 %
@Temperature -182 °C
52 %
@Temperature -296 °F
 60 %
@Temperature 427 °C
60 %
@Temperature 801 °F
Reduction of Area  27 %
@Temperature 316 °C
27 %
@Temperature 601 °F
 32 %
@Temperature 204 °C
32 %
@Temperature 399 °F
 33 %
@Temperature 538 °C
33 %
@Temperature 1000 °F
 51 %
@Temperature -182 °C
51 %
@Temperature -296 °F
 55 %
@Temperature 427 °C
55 %
@Temperature 801 °F
 56 %
@Temperature -29.0 °C
56 %
@Temperature -20.2 °F
 56 %
@Temperature 20.0 °C
56 %
@Temperature 68.0 °F
 57 %
@Temperature -60.0 °C
57 %
@Temperature -76.0 °F
Modulus of Elasticity 115 GPa16700 ksi
 45.0 GPa
@Temperature 538 °C
6530 ksi
@Temperature 1000 °F
 67.0 GPa
@Temperature 427 °C
9720 ksi
@Temperature 801 °F
 81.0 GPa
@Temperature 316 °C
11700 ksi
@Temperature 601 °F
 130 GPa
@Temperature 204 °C
18900 ksi
@Temperature 399 °F
 136.5 GPa
@Temperature 20.0 °C
19800 ksi
@Temperature 68.0 °F
 139 GPa
@Temperature -182 °C
20200 ksi
@Temperature -296 °F
 172 GPa
@Temperature -29.0 °C
24900 ksi
@Temperature -20.2 °F
 176.5 GPa
@Temperature -60.0 °C
25600 ksi
@Temperature -76.0 °F
Poissons Ratio 0.3120.312
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Charpy Impact 81.0 - 88.0 J59.7 - 64.9 ft-lbKeyhole, temper not reported
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000123 ohm-cm
@Temperature 20.0 °C
0.0000123 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 56.5 W/m-K392 BTU-in/hr-ft²-°F
Melting Point 1040 - 1045 °C1900 - 1913 °F
Solidus 1040 °C1900 °F
Liquidus 1045 °C1913 °F
Annealing Point 607.2 - 899 °C1125 - 1650 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 1010 °C1850 °FHot-Shortness Temperature
Annealing Temperature 600 - 900 °C1110 - 1650 °F
Hot-Working Temperature 800 - 925 °C1470 - 1700 °F
Recrystallization Temperature 785 - 870 °C1450 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 - 8.0 %6.0 - 8.0 %
Copper, Cu 88 - 92.5 %88 - 92.5 %
Iron, Fe 1.5 - 3.5 %1.5 - 3.5 %
Lead, Pb <= 0.010 %<= 0.010 %
Manganese, Mn <= 1.0 %<= 1.0 %
Other, total <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.015 %<= 0.015 %
Zinc, Zn <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C61300, Annealed
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
8% Aluminum Bronze, UNS C61000
Aluminum bronze 5%, UNS C60800
Ampco Metal AMPCO® 45 Nickel-Aluminum Bronze, Extruded and Drawn Rods, ≤ 25.4 mm.

MC61400c8 / 171644

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.