MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolene® HB6007 Blow Molding HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Homopolymer

Applications: Milk, distilled water, soft drink concentrate, fruit juice, etc.

Formolene HB6007 is a high quality product for those critical food packaging requirements. It also has excellent stiffness and good stiffness properties.

Produced using licensor formulation for EHM 6007. Licensor does not warrant or imply that this product meets their specifications for EHM 6007.

Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.964 g/cc0.0348 lb/in³ASTM D1505
Environmental Stress Crack Resistance 10 hour10 hourCondition B, F50; ASTM D1693
ESCR 100% Igepal® 15 - 20 hour15 - 20 hourCondition A, F50; ASTM D1693
Melt Flow 0.65 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.3 MPa4400 psi2" (50mm) per min.; ASTM D638 Type IV
Elongation at Break >= 300 %>= 300 %2" (50mm) per min.; ASTM D638 Type IV
Flexural Modulus 1.65 GPa240 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -118 °C<= -180 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese GUR® 2122 PE-UHMW, Specialty
Bamberger Polymers Bapolene® 0760 High Density Polyethylene, Blow Molding Grade
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
Formosa Plastics Formolene® HB5502F Blow Molding HDPE
ExxonMobil Paxon™ BA50-100 Blow Molding Resin

PFPCPE11 / 38818

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.