MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

MOL Group TIPOLEN 245-51 LDPE, Injection and Extruded
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade; Low Density Polyethylene (LDPE), Molded

Material Notes: Description: TIPOLEN EE 245-51 is a low density polyethylene copolymer intended mainly for extrusion and injection molding applications where a combination of good processability with enhanced thermal resistance and a product toughness with lower stiffness are required. Through better adhesion it shows moderate compatibility with glass, metal, paint and other polar materials. This grade is additives free.

Applications: TIPOLEN EE 245-51 is recommended for thin wall injection molding, coating of parts and pipes, soft profiles and sheets, compounding.

(1) Density, Vicat Softening Temperature and Shore D Hardness have been measured on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). (2) Average mechanical property values of several measurements carried out on standard injection-molded test specimens prepared in accordance with ISO 294-1.

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³1; ISO 1183-1
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 46461; ISO 868
Tensile Strength 10.0 MPa1450 psi2; ISO 527-1,2
Elongation at Break 164 %164 %2; ISO 527-1,3
Flexural Modulus 0.200 GPa29.0 ksi2; ISO 178
Izod Impact, Notched (ISO) 42.0 kJ/m²20.0 ft-lb/in²2; ISO 180/A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 85.0 °C185 °F1; ISO 306/A 120
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 220 °C320 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG018 / 297184

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.